Electrode
Counter electrodes
We offer several materials and size for the counter electrodes. When choosing the counter electrode care must be taken in the electrode area, which should not be lower than the working electrode area, otherwise the counter becomes a limiting factor for the flowing current. The counter electrodes are divided in two categories: small and large, the same way the reference electrodes or the cells are divided.
Specifications
| Catalog No. | Material | Mesh | Dimensions/cm | Wire Ø/mm | Surf. Area/cm² | Purpose |
A-002222![]() | Pt wire | N/A | 5.7 | 0.5 | ~ 0.7 | SVC-2, VC-4, plate material evaluating cell |
| A-002233 | Pt wire with PEEK | N/A | 5 | 0.5 | ~ 0.7 | SVC-3 |
| A-002234 | Pt coil | N/A | 4.5 (23 coiled) | 0.5 | ~ 3.6 | RRDE-3A, bulk electrolysis, SVC-3 |
| A-012638 | Au | N/A | 4.5 (23 coiled) | 0.5 | ~ 3.6 | RRDE-3A, bulk electrolysis, SVC-3 |
| A-012639 | Ni | N/A | 4.5 (23 coiled) | 0.5 | ~ 3.6 | RRDE-3A, bulk electrolysis, SVC-3 |
A-002250![]() | Pt gauze electrode with PEEK | 80 | 2.5 x 3.5 | 0.08 | ~ 22.9 | |
| A-702439 | Pt wire 54 mm | 80 | 2.5 x 3.5 | 0.08 | ~ 22.9 | Flat cell |
A-013612![]() | Pt gauze electrode | 80 | height : 5 Ø : 4 | 0.12 | ~ 47.4 | Bulk electrolysis |
| A-002251 | Au gauze electrode with PEEK | 100 | 2.5 x 3.5 | 0.07 | ~ 29 | |
| A-010530 | Carbon | N/A | height: 5.5 ID : 3 OD : 3.8 | 0.5 | 10.5 cm²/cm³ | Bulk electrolysis |