Corrosion Cell
Flat cells
A cell designed for to study corrosion on flat samples
The flat cell is a double-jacketed 250 mL cell designed to perform standard corrosion experiments on large flat samples of any size with a maximum thickness of 6 mm. The exposed area can be 1 or 10 cm².
This cell has a double jacket for temperature control and three ports for a reference electrode, a purge tube, to control the gaseous environment of the cell, and a temperature probe. It is provided with a platinum mesh counter electrode and a bridge tube for the reference electrode. It is available for exposed sample area of 1 and 10 cm².
Specifications and ordering information
Sample size
- Min diameter: 30.5 mm (EL-FLAT-1CM); 40.5 mm (EL-FLAT-10CM)
- Max. thickness: 6 mm
Inner diameters of the ports: 17.6 mm x 1; 8.3 mm x 2
EL-FLAT-1CM | EL-FLAT-10CM |
|
| Platinum gauze counter electrode | ||
| Bridge tube for ref. electrode (6 mm diameter) | ||
| Glass cell for flat cell (250 mL) Double jacket. | ||
| Mechanical parts | ||
EL-FLAT-1CM-PVDF | EL-FLAT-10CM-PVDF |
|
| Platinum gauze counter electrode | ||
| Bridge tube for ref. electrode (6 mm diameter) | ||
| Glass cell for flat cell (250 mL) Single jacket. | ||
| Mechanical parts | ||
Related topics